We will respond patiently and carefully to any inquiries and feedback from customers; For any inquiry from customers, we will provide professional and reasonable quotations as soon as possible.
We will respond patiently and carefully to any inquiries and feedback from customers; For any inquiry from customers, we will provide professional and reasonable quotations as soon as possible.
The current payment methods for foreign trade orders are T/T and L/C. If the order amount is less than 1,000 US dollars, the full amount must be paid before the order; if the order amount is greater than 1,000 US dollars, 30% must be paid before the order is made, and the balance must be paid before shipment; in other cases, Specific discussions;
The payment method for domestic orders is determined based on specific circumstances.
Foreign trade orders are basically shipped by sea. We are close to Ningbo Port and Shanghai Port, and shipping exports are very convenient. If the customer's goods are urgent, we can also transport them by air. Hangzhou Xiaoshan Airport is also relatively close to us;
Domestic orders are shipped through two methods: logistics and chartered vehicles, which are determined based on the specific order.
Cause analysis and suggested solutions
(1) The amount of ink is too large and the paper cannot bear it —— Replace high-weight paper;
(2) The printing environment is too dry —— The printing environment humidity is controlled at 45%-65% between;
(3) Rewinder tension is too high —— Adjust the winding tension as appropriate;
(4) The elastic edges of the paper make the paper feeding unstable —— Increase loose edge tension or change paper.
Cause analysis and suggested solutions
( 1 ) The unwinding tension on both sides of the transfer machine is inconsistent —— Adjust the tension of the transfer machine to keep the tension on both sides consistent;
( 2 ) Transfer machine blanket pressure is insufficient —— Increase blanket pressure;
( 3 ) The backing paper or fabric is wrinkled —— Cut off the existing transfer backing paper and fabric and re-transfer;
( 4 ) The elastic edge of the paper makes the paper feeding unstable. —— Increase the unwinding tension on the loose side of the transfer machine. If the transfer machine cannot adjust the tension on one side, the loose side tension can be artificially increased;
( 5 )The fabric is too thick and has poor breathability —— Slow down the transfer speed.
Cause analysis and suggested solutions
(1) Printer nozzle clogged —— Clean the nozzle or replace the nozzle;
(2) Uneven coating of paper —— Replace paper;
(3) Displacement caused by printing arching —— Replace paper with higher weight or faster drying speed;
(4) Inconsistent coating on paper base —— Use the same model product;
(5) Transfer conditions are inconsistent —— Unified transfer conditions ;
(6) The storage time of printed paper varies greatly. —— Keep the storage time basically the same.
Cause analysis and suggested solutions
(1) The amount of ink is too large and has not been dried. —— Replace products with higher weight or increase drying intensity;
(2) The storage environment is too humid and the printed paper will get damp. —— Store the printed products in a sealed plastic bag;
(3) The ink used is easy to sublimate —— Control the printing environment temperature and storage temperature. It is recommended to be lower than 30 degrees Celsius;
(4) There are liquid drops on the paper during the printing and rewinding process. —— Clean printing equipment promptly.
Cause analysis and suggested solutions
(1) Paper gets damp —— Replace paper and control the humidity of product storage environment 45%-65% ;
(2) Paper moisture content is low —— Adjust the humidity of the printing environment, and pre-expose the paper to the environment before printing to balance the moisture of the paper;
(3) The paper used is too rough, resulting in reduced clarity —— Replace the paper and use a smoother product.
(4) The amount of printing ink is too large and the paper cannot absorb it. —— Replace with higher weight products.
Cause analysis and suggested solutions
(1) Scratch defects during coating process —— Replace paper;
(2) Bruises and scratches during the cutting process —— Replace paper;
(3) The paper feed roller is scratched during printing —— Clean the printing equipment and replace the paper ;
Cause analysis and suggested solutions
(1) Oil stains: Generally larger, can be inked —— Replace paper;
(2) Water dots: regular small dots that do not completely leak out after printing —— Replace paper;
(3) Dust: extremely fine, completely leaking —— Replace the paper.
During the printing process, the drying temperature is too high, causing the paper fibers to lose water, deform and arch.
(1) In an environment where the room temperature is 20~35℃ and the humidity is 40~60%, the printing platform heating can be turned off or turned on at a lower temperature to prevent the paper from arching due to water loss;
(2) Reduce the air suction force on the printer table as much as possible. Especially when stopping printing, please turn off the air suction on the table to prevent some paper left on the table from being wrinkled.
High ambient humidity leads to sticky powder; low ambient humidity leads to static sticky powder.
(1) When the humidity of the powder shaking environment is greater than 80%, turn on the dehumidifier or turn on the front guide plate heating of the powder shaking machine to prevent powder from sticking due to moisture absorption on the surface;
(2) When the humidity of the powder shaking environment is less than 40%, turn on the humidifier, and touch the powder shaking machine with your hands to reduce static electricity when the powder shaking machine is powered off.
If the temperature is too high, the pattern will lose too much water, resulting in insufficient adhesion of the hot melt powder.
Turn off the table heating when printing and turn off the front plate heating of the toner shaker.
(1) Shake the powder lightly depending on the state of the hot-melt powder;
(2) Select the appropriate drying temperature according to the selected hot melt adhesive to ensure that the hot melt adhesive powder is completely melted.
Due to the weather, the room temperature is too low or the air humidity is too high, causing the white ink to dry slowly, resulting in the ink layer containing more water. The water remains in the ink layer during drying after shaking, and turns into water vapor during hot stamping. The pattern appears with more white spots.
This can be solved by increasing the heating temperature of the printer and shaker guide plates to properly evaporate the water in the ink layer.
(1) Determine the accurate transfer temperature, pressure and time based on different fabrics, heat transfer machines, and hot melt adhesive powder. You can do a small trial with the same fabric before formal mass production to determine the hot stamping method that achieves satisfactory product results. temperature and time. For recommended conditions for related materials, please refer to the instructions of our products;
(2) Stretch fabrics must be preheated before transfer.
(1) When using, select the appropriate peeling speed (cold tearing, hot tearing and second tearing) according to the properties of the fabric and hot melt adhesive powder;
(2) It supports cold tearing and hot tearing. When using instant tearing, the action should be as fast as possible. Slow tearing may cause edge warping.